ꯇꯦꯜ: +꯸꯶ 15221953351 ꯏ-ꯃꯦꯜ: info@herchyrubber.com
Please Choose Your Language
PRODUCTS ꯒꯤ ꯃꯇꯥꯡꯗꯥ ꯋꯥꯐꯝ ꯀꯌꯥ ꯊꯃꯈꯤ꯫
ꯑꯗꯣꯝ ꯃꯐꯝ ꯑꯁꯤꯗꯥ ꯂꯩꯔꯤ: ꯌꯨꯝ » ꯄꯣꯠꯊꯣꯀꯁꯤꯡ꯫ » ꯁꯤꯟꯊꯦꯁꯤꯁ ꯔꯕ꯭ꯕꯔ꯫ » ꯚꯤ.ꯑꯦꯝ.ꯀ꯭ꯌꯨ.ꯒꯤ ꯁꯤꯂꯤꯀꯣꯟ꯫ » ꯖꯤ.ꯑꯦ.-꯵꯷ꯑꯦꯛꯁ.ꯑꯦꯛꯁ.ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯔꯣꯂꯔ ꯁꯤꯂꯤꯀꯣꯟ ꯔꯕ꯭ꯕꯔ (ꯑꯩꯆ.ꯁꯤ.ꯑꯥꯔ.)

ꯂꯣꯗ ꯇꯧꯕꯥ꯫

ꯁꯦꯌꯔ ꯇꯧꯕꯤꯌꯨ:
ꯐꯦꯁꯕꯨꯛ ꯁꯦꯌꯔ ꯇꯧꯕꯒꯤ ꯕꯣꯇꯥꯝ꯫
ꯇ꯭ꯕꯤꯇꯔ ꯁꯦꯌꯔ ꯇꯧꯕꯒꯤ ꯕꯇꯟ꯫
ꯂꯥꯏꯟ ꯁꯦꯌꯔ ꯇꯧꯕꯒꯤ ꯕꯇꯟ꯫
ꯋꯦꯆꯦꯠ ꯁꯦꯌꯔ ꯇꯧꯕꯒꯤ ꯕꯇꯟ꯫
ꯂꯤꯉ꯭ꯀꯗꯤꯟ ꯁꯦꯌꯔ ꯇꯧꯕꯒꯤ ꯕꯇꯟ꯫
pinterest ꯁꯦꯌꯔ ꯇꯧꯕꯥ ꯕꯇꯟ꯫
whatsapp ꯁꯦꯌꯔ ꯇꯧꯕꯒꯤ ꯕꯣꯇꯥꯝ꯫
ꯁꯦꯌꯔ ꯇꯧꯕꯒꯤ ꯕꯇꯟ ꯑꯁꯤ ꯁꯦꯌꯔ ꯇꯧꯕꯤꯌꯨ꯫

ꯖꯤ.ꯑꯦ.-꯵꯷ꯑꯦꯛꯁ.ꯑꯦꯛꯁ.ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯔꯣꯂꯔ ꯁꯤꯂꯤꯀꯣꯟ ꯔꯕ꯭ꯕꯔ (ꯑꯩꯆ.ꯁꯤ.ꯑꯥꯔ.)

ꯖꯤ.ꯑꯦ.-꯵꯷ꯑꯦꯛꯁ.ꯑꯦꯛꯁ.ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯔꯣꯂꯔ ꯁꯤꯂꯤꯀꯣꯟ ꯔꯕ꯭ꯕꯔ (ꯑꯩꯆ.ꯁꯤ.ꯑꯥꯔ.)
 
ꯑꯦꯞꯂꯤꯀꯦꯁꯟ: ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯀꯣꯠ, ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯄ꯭ꯂꯦꯠ, ꯍꯣꯠ ꯇ꯭ꯔꯥꯟꯁꯐꯔ ꯔꯣꯂꯔ, ꯀꯣꯄꯤꯔ ꯔꯣꯂꯔ,ꯅꯆꯤꯡꯕꯥ ꯄꯨꯊꯣꯀꯄꯗꯥ ꯆꯨꯅꯕꯥ꯫
 
ꯃꯔꯨꯑꯣꯏꯕꯥ ꯃꯁꯀꯁꯤꯡ: ꯑꯋꯥꯡꯕꯥ ꯑꯃꯁꯨꯡ ꯅꯦꯝꯕꯥ ꯇꯦꯝꯄꯦꯔꯦꯆꯔꯗꯥ ꯑꯐꯕꯥ ꯔꯦꯁꯤꯁ꯭ꯇꯦꯟꯁ (60 'C -350 'C), ꯑꯋꯥꯡꯕꯥ ꯔꯦꯁꯤꯂꯤꯌꯦꯟꯁ ꯑꯃꯁꯨꯡ ꯑꯐꯕꯥ ꯑꯦꯕꯔꯦꯁꯟ ꯔꯦꯁꯤꯁ꯭ꯇꯦꯟꯁ,ꯂꯣ ꯗꯤꯐꯣꯔꯃꯦꯁꯟ ꯁꯦꯠ, ꯍꯥꯔꯗ ꯇꯨ ꯗꯤꯐꯣꯔꯃꯦꯁꯟ ꯑꯃꯁꯨꯡ ꯐ꯭ꯔꯦꯀꯆꯔ, ꯁꯥꯡꯅꯥ ꯁꯔꯚꯤꯁ ꯂꯥꯏꯐ꯫
  • ꯖꯤ.ꯑꯦ.-꯵꯷ꯑꯦꯛꯁ.ꯑꯦꯛꯁ.ꯇꯥ ꯂꯩ꯫

  • ꯍꯔꯆꯤ꯫

ꯐꯪꯒꯗꯕꯥ:
ꯃꯁꯤꯡ: ꯱.
ꯖꯤ.ꯑꯦ.-꯵꯷ꯑꯦꯛꯁ.ꯑꯦꯛꯁ.ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯔꯣꯂꯔ ꯁꯤꯂꯤꯀꯣꯟ ꯔꯕ꯭ꯕꯔ (ꯑꯩꯆ.ꯁꯤ.ꯑꯥꯔ.)


ꯑꯦꯞꯂꯤꯀꯦꯁꯟ: ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯀꯣꯠ, ꯍꯣꯠ ꯁ꯭ꯇꯦꯝꯄꯤꯡ ꯄ꯭ꯂꯦꯠ, ꯍꯣꯠ ꯇ꯭ꯔꯥꯟꯁꯐꯔ ꯔꯣꯂꯔ, ꯀꯣꯄꯤꯔ ꯔꯣꯂꯔ,ꯅꯆꯤꯡꯕꯥ ꯄꯨꯊꯣꯀꯄꯗꯥ ꯆꯨꯅꯕꯥ꯫

ꯃꯔꯨꯑꯣꯏꯕꯥ ꯃꯁꯀꯁꯤꯡ: ꯑꯋꯥꯡꯕꯥ ꯑꯃꯁꯨꯡ ꯅꯦꯝꯕꯥ ꯇꯦꯝꯄꯦꯔꯦꯆꯔꯗꯥ ꯑꯐꯕꯥ ꯔꯦꯁꯤꯁ꯭ꯇꯦꯟꯁ (60 'C -350 'C), ꯑꯋꯥꯡꯕꯥ ꯔꯦꯁꯤꯂꯤꯌꯦꯟꯁ ꯑꯃꯁꯨꯡ ꯑꯐꯕꯥ ꯑꯦꯕꯔꯦꯁꯟ ꯔꯦꯁꯤꯁ꯭ꯇꯦꯟꯁ,ꯂꯣ ꯗꯤꯐꯣꯔꯃꯦꯁꯟ ꯁꯦꯠ, ꯍꯥꯔꯗ ꯇꯨ ꯗꯤꯐꯣꯔꯃꯦꯁꯟ ꯑꯃꯁꯨꯡ ꯐ꯭ꯔꯦꯀꯆꯔ, ꯁꯥꯡꯅꯥ ꯁꯔꯚꯤꯁ ꯂꯥꯏꯐ꯫

ꯇꯦꯁ꯭ꯠ ꯇꯧꯕꯥ: ꯀ꯭ꯌꯨꯔꯤꯡ ꯑꯦꯖꯦꯟꯇꯀꯤ ꯱% (ꯁꯤꯂꯤꯀꯣꯟ ꯒꯃꯗꯥ ꯗꯤ.ꯕꯤ.ꯄꯤ.ꯑꯦꯝ.ꯑꯩꯆ.ꯒꯤ ꯵꯰% ꯄꯦꯁ꯭ꯠ),꯱꯷꯵'ꯁꯤ x ꯵ꯃꯤꯅꯤꯠ x ꯱꯵ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.



ꯄ꯭ꯔꯗꯛꯇ ꯄꯦꯔꯥꯃꯤꯇꯔꯁꯤꯡ꯫


ꯄꯣꯠꯊꯣꯛ ꯖꯤ.ꯑꯦ.-꯵꯷꯵꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ ꯖꯤ.ꯑꯦ.-꯵꯷꯷꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ ꯖꯤ.ꯑꯦ.-꯵꯷꯸꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ ꯖꯤ.ꯑꯦ.-꯵꯷꯴꯱ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ ꯖꯤ.ꯑꯦ.-꯵꯷꯶꯱ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫
ꯃꯄꯥꯟꯊꯣꯡꯗ ꯎꯕ ꯍꯣꯌꯤ꯫ ꯐꯦꯠ ꯌꯦꯜꯂꯣ꯫
ꯍꯥꯔꯗꯅꯦꯁ (ꯁꯣꯔꯑꯦ) ꯑꯃꯁꯨꯡ ꯑꯦꯟ. 55 70 80 43 60
ꯇꯦꯟꯁꯥꯏꯜ ꯁ꯭ꯠꯔꯦꯡꯊ (ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.) ꯑꯃꯁꯨꯡ ꯑꯦꯝ.ꯄꯤ.ꯑꯦ. 5.5 6 7 6 8
ꯏꯂꯣꯡꯒꯦꯁꯟ(%) ꯴. 230 150 100 400 350
ꯇꯤꯌꯥꯔ ꯁ꯭ꯠꯔꯦꯡꯊ (kN/m) ꯑꯁꯤꯅꯤ꯫ 10 9 9 15 25
꯱꯷꯵'ꯁꯤ x꯲꯲h ꯀꯝꯞꯔꯦꯁꯟ(%) 8 10 10 10 10


ꯃꯃꯥꯡꯒꯤ: 
ꯃꯊꯪ: 

ꯃꯔꯤ ꯂꯩꯅꯕꯥ ꯄ꯭ꯔꯗꯛꯇ ꯔꯤꯀꯃꯦꯟꯗꯦꯁꯟ꯫

QUICK LINKS ꯇꯧꯕꯥ꯫

ꯀꯟꯇꯦꯛꯇꯀꯤ ꯏꯅꯐꯣꯔꯃꯦꯁꯟ꯫

ꯍꯥꯄꯆꯤꯅꯕꯥ: ꯅꯪ.꯳꯳, ꯂꯦꯟ ꯱꯵꯹, ꯇꯥꯏꯌꯦ ꯔꯣꯗ, ꯐꯦꯡꯁꯤꯌꯥꯟ ꯗꯤꯁ꯭ꯠꯔꯤꯛꯇ, ꯁꯉ꯭ꯒꯣꯝ꯫
ꯇꯦꯜ / ꯋꯥꯇꯁꯑꯦꯞ / ꯁ꯭ꯀꯥꯏꯞ: +꯸꯶ 15221953351
ꯏ-ꯃꯦꯜ: ꯱.  info@herchyrubber.com
ꯀꯥꯄꯤꯔꯥꯏꯠ     2023 ꯁꯉ꯭ꯒꯣꯝ ꯍꯔꯆꯤ ꯔꯕ꯭ꯕꯔ ꯀꯣꯡ, ꯂꯤꯃꯤꯇꯦꯗ꯫ ꯁꯥꯏꯇꯃꯦꯞ ꯇꯧꯕꯥ꯫ |   ꯄ꯭ꯔꯥꯏꯕꯦꯁꯤ ꯄꯣꯂꯤꯁꯤ | ꯁꯄꯣꯔꯠ ꯕꯥꯏ... ꯂꯤꯗꯣꯡ꯫.