GA-91X3B High ọkwa antistatic silicone roba (nwa) (HCR)

Ngwa: adabara amị antistatic silicone rollers, antistatic gasket, mobile fixtures, ulo oru iche iche wdg.
Njirimara ndị dị mkpa: Enwere ike idowe ihe mgbochi na-adịgide adịgide, na-egbochi ịsa mmiri dị elu, gafere nyocha nke RoHS na REACH.
  • GA-91X3B

  • Herchy

Nnweta:
Ọnụọgụ:

Nnwale: 1% nke onye na-agwọ ọrịa (50% tapawa nke DBPMH na silicone gum), 175° x5minx15MPa


Ngwa ngwaahịa
Ngwaahịa GA-9153B GA-9163B GA-9173B GA-9183B
Ọdịdị Nwa
Isi ike (ShoreA)
50
60
70
80
Njupụta (g/cm3) 1.16
1.18
1.21
1.22
Ike tensile (MPa)

9.0
8.0
7.0
7.0
Mgbatị(%) 500
400
300
150
Ike akwa mmiri (kN/m) 20
20
16
16
Nguzogide elu (Ω) 105--106









Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.