GA-97XX Mmanụ na-eguzogide silicone rọba (HCR)

GA-97XX Mmanụ na-eguzogide silicone rọba (HCR)
Ngwa: adabara maka mmepụta nke ngwaahịa na-eguzogide mmanụ.
Ihe ndị dị mkpa: ike dị elu, ezigbo ndidi na ASTM 1 # na mmanụ IRM903, nyefee nkwenye nke RoHS na REACH.
 
  • GA-97XX

  • Herchy

Nnweta:
Ọnụọgụ:

GA-97XX Mmanụ na-eguzogide silicone rọba (HCR)


Ngwa: adabara maka mmepụta nke ngwaahịa na-eguzogide mmanụ.
Njirimara ndị dị mkpa: ike dị elu, ezigbo ndidi na ASTM 1 # na mmanụ IRM903, gafere nkwenye nke RoHS na REACH.
Nnwale: 1% nke onye na-agwọ ọrịa (50% tapawa nke DBPMH na silicone gum), 175°Cx5min x15MPa.



Ngwa ngwaahịa
Ngwaahịa GA-9740 GA-9750 GA-9760 GA-9770
Ọdịdị Agba ntụ
Williamplasticity 140 180 200 260
Isi ike (ShoreA) 40 50 60 70
Njupụta (g/cm3) 1.23 1.25 1.28 1.32
Ike tensile (MPa) 3.5 4.5 5 5.5
Mgbatị(%) 700 600 400 250
Ike akwa mmiri (kN/m) 15 15 15 15
175'C x22h mkpakọ(%) 20 20 20 20
Ikuku ịka nká 225°C x70H Isi ike na-agbanwe 1 2 2 2
Ọnụego mgbanwe ike ụjọ -25% -25% -25% -25%
Ọnụego mgbanwe elongation -30% -30% -30% -30%
Mmanụ IRM903 150°C x70H Isi ike na-agbanwe -18 -18 -17 -16
Ọnụego mgbanwe ike ụjọ -35% -35% -35% -35%
Ọnụego mgbanwe elongation -20% -20% -20% -20%
Mgbanwe olu 36% 36% 35% 35%


Nke gara aga: 
Osote: 

Njikọ ngwa ngwa

Ngwaahịa anyị

OZI MKPỌTỤRỤ

Tinye: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Nwebiisinka     2023 Shanghai Herchy Rubber Co., Ltd. map saịtị |   Amụma nzuzo | Nkwado Site Leadong.