GA-91X3B jedhamuun beekama
Herchy jedhamuun beekama
| Argamuu: | |
|---|---|
| Baay'ina: | |
Qormaata: %1 kan fayyisu (%50 paastaa DBPMH silikoonii gogaa keessatti), 175° x5minx15MPa
| Parameetaroota oomishaa | ||||
| Oomisha | GA-9153B irratti kan argamu | GA-9163B irratti kan argamu | GA-9173B jedhamuun kan beekamu | GA-9183B jedhamuun kan beekamu |
| Mul'ina | Gurraacha | |||
| Jabina (ShoreA) . |
50 |
60 |
70 |
80 |
| Dandeettii(g/cm3) . | 1.16 |
1.18 |
1.21 |
1.22 |
| Jabina harkisaa (MPa) . |
9.0 |
8.0 |
7.0 |
7.0 |
| Dheersuu(%) . | 500 |
400 |
300 |
150 |
| Jabina ciccituu (kN/m) . | 20 |
20 |
16 |
16 |
| Diddaa fuula(Ω) . | 105--106 | |||