GA-91X3B
Herchy
| Availability: | |
|---|---|
| Quantitas: | |
Test: 1% curationis agentis (50% crustulum DBPMH in gummi siliconis), 175° x5minx15MPa
| Product parametri | ||||
| Productum | GA-9153B | GA-9163B | GA-9173B | GA-9183B |
| Aspectus | Niger | |||
| Duritia (ShoreA) |
50 |
60 |
70 |
80 |
| Densitas (g/cm3) | 1.16 |
1.18 |
1.21 |
1.22 |
| Roboris distrahentes (MPa) |
9.0 |
8.0 |
7.0 |
7.0 |
| Prolongatio(%) | 500 |
400 |
300 |
150 |
| Robur scindere (kN/m) | 20 |
20 |
16 |
16 |
| Superficies resistentia (Ω) | 105--106 | |||