ꯖꯤ.ꯑꯦ.-꯹꯱ꯑꯦꯛꯁ꯳ꯕꯤ
ꯍꯔꯆꯤ꯫
| ꯐꯪꯒꯗꯕꯥ: | |
|---|---|
| ꯃꯁꯤꯡ: ꯱. | |
ꯇꯦꯁ꯭ꯠ ꯇꯧꯕꯥ: ꯀ꯭ꯌꯨꯔꯤꯡ ꯑꯦꯖꯦꯟꯇꯀꯤ 1% (ꯁꯤꯂꯤꯀꯣꯟ ꯒꯃꯗꯥ DBPMHꯒꯤ 50% ꯄꯦꯁ꯭ꯠ), 175° x5minx15MPa꯫
| ꯄ꯭ꯔꯗꯛꯇ ꯄꯦꯔꯥꯃꯤꯇꯔꯁꯤꯡ꯫ | ||||
| ꯄꯣꯠꯊꯣꯛ | ꯖꯤ.ꯑꯦ.-꯹꯱꯵꯳ꯕꯤ | ꯖꯤ.ꯑꯦ.-꯹꯱꯶꯳ꯕꯤ | ꯖꯤ.ꯑꯦ.-꯹꯱꯷꯳ꯕꯤ | ꯖꯤ.ꯑꯦ.-꯹꯱꯸꯳ꯕꯤ |
| ꯃꯄꯥꯟꯊꯣꯡꯗ ꯎꯕ | ꯑꯃꯨꯕ | |||
| ꯍꯥꯔꯗꯅꯦꯁ (ꯁꯣꯔꯑꯦ) ꯑꯃꯁꯨꯡ ꯑꯦꯟ. |
50 |
60 |
70 |
80 |
| ꯗꯦꯟꯁꯤꯇꯤ(ꯖꯤ/ꯁꯦ.ꯃꯤ.꯳) ꯑꯁꯤꯅꯤ꯫ | 1.16 |
1.18 |
1.21 |
1.22 |
| ꯇꯦꯟꯁꯥꯏꯜ ꯁ꯭ꯠꯔꯦꯡꯊ (ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.) ꯑꯃꯁꯨꯡ ꯑꯦꯝ.ꯄꯤ.ꯑꯦ. |
9.0 |
8.0 |
7.0 |
7.0 |
| ꯏꯂꯣꯡꯒꯦꯁꯟ(%) ꯴. | 500 |
400 |
300 |
150 |
| ꯇꯤꯌꯥꯔ ꯁ꯭ꯠꯔꯦꯡꯊ (kN/m) ꯑꯁꯤꯅꯤ꯫ | 20 |
20 |
16 |
16 |
| ꯁꯔꯐꯦꯁ ꯔꯦꯁꯤꯁ꯭ꯇꯦꯟꯁ(Ω) ꯑꯁꯤꯅꯤ꯫ | 105--꯱꯰6 | |||