Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 8.5%
Ethylene content: 72%
Oil content:100%
Mooney viscosity: ML(1+4)125°C 47
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 9.4%
Ethylene content: 55%
Mooney viscosity: ML(1+4)125°C 29
Size: 25kg/block
MOQ: 25kg
Packing: boxed