Molekyule mu duru a ɛkorɔn yiye Ethylene Propylene
Sɛnea ɛte ne tebea: fitaa (ɛda adi anaasɛ ɛyɛ hann) blocky
Monomer a ɛto so abiɛsa ne nea ɛwɔ mu: ENB, 8.5%
Ethylene dodow: 72%
Ngo dodow:100%
Mooney viscosity: ML(1+4)125°C 47
Kɛse: 25kg/block
MOQ: 25kg
Packing: boxed