ʻO ka hiʻohiʻona a me ke kūlana: keʻokeʻo (transparent a translucent) blocky
ʻO ke ʻano monomer ʻekolu a me ka ʻike: ENB, 5.7%
Ethylene maʻiʻo: 58%
Mooney viscosity: ML (1 + 4) 125 ° C 84
Nui: 25kg / poloka
MOQ: 25kg
Hoʻopili: pahu pahu
ʻO ke ʻano a me ke kūlana: keʻokeʻo (transparent a translucent) blocky
ʻO ke ʻano monomer ʻekolu a me ka maʻiʻo: ENB, 8.5%
Ethylene maʻiʻo: 72%
ʻaila ʻaila: 100%
Mooney viscosity: ML(1+4)125°C 47
Nui: 25kg/block
MOQ: 25kg
Pākuʻi: pahu