Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 1.0%
nilalaman ng ethylene: 66%
Mooney Viscosity: ML (1+4) 125 ° C 46
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 8.5%
nilalaman ng etilena: 72%
nilalaman ng langis : 100%
viscosity ng mooney: ml (1+4) 125 ° C 47
laki: 25kg/block
moq: 25kg
packing: boxed