Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 2.3%
Ethylene content: 57%
Mooney viscosity: ML(1+4)125°C 35
Size: 25kg/block
MOQ: 25kg
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 5.5%
Ethylene content: 68%
Mooney viscosity: ML(1+4)125°C 87
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 4.5%
Ethylene content: 69%
Mooney viscosity: ML(1+4)125°C 63
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 6.5%
Ethylene content: 68%
Mooney viscosity: ML(1+4)125°C 135
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 1.0%
Ethylene content: 66%
Mooney viscosity: ML(1+4)125°C 46
Size: 25kg/block
MOQ: 25kg
Packing: boxed