A ɲɛda ni a cogoya: fin (transparent walima translucent) Blocky
sabanan monomɛri suguya ani a kɔnɔkow: ENB, 2,3%
etilɛni hakɛ: 57%
Mooney Viscosité: ml(1+4)125°C 35
A bonya: 25kg/block
MOQ: 25kg
A ɲɛda ni a cogoya: fin (transparent walima translucent) Blocky
sabanan monomɛri suguya ani a kɔnɔkow: ENB, 9,4%
etylene hakɛ: 55%
Mooney Viscosity: ml(1+4)125°C 29
A bonya: 25kg/block
MOQ: 25kg
Packing: Boxed