Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 8.5%
Ethylene content: 72%
Te hinu hinu: 100%
Mooney viscosity: ML(1+4)125°C 47
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka
Te ahua me te ahua: ma (maamaa ranei) poraka
Tuatoru momo monomer me te ihirangi: ENB, 9.4%
Ethylene ihirangi: 55%
Mooney viscosity: ML(1+4)125°C 29
Rahi: 25kg/poraka
MOQ: 25kg
Te takai: pouaka