Pammarang ken Kasasaad: Puraw (Transparent wenno Translucent) Naserraan
a maikatlo a kita ti monomero ken linaon: ENB, 4.1%
Etileno Linaon: 58%
Mooney Viscosity: ML(1+4)125°C 84
Size: 25kg/block
MOQ: 25kg
Packing: Nakakahon a nakakahon
Pammarang ken Kasasaad: Puraw (Transparent wenno Translucent) Naserraan
a maikatlo a kita ti monomero ken linaon: ENB, 5.7%
Etileno Linaon: 58%
Mooney Viscosity: ML(1+4)125°C 84
Kadakkel: 25kg/block
MOQ: 25kg
Packing: Nakakahon a nakakahon