GA-9442
I-Herchy
| Ukutholakala: | |
|---|---|
| Ubuningi: | |
Ukuhlolwa: I-DBPMH, ukuphulukiswa kokuqala: 170°C x 10min, ukuphulukiswa kokuthunyelwe.200°C x4H.
| Imingcele yomkhiqizo | ||
| Umkhiqizo | GA-9442 |
GA-9443 |
| Ukubukeka | ophuzi ophelile |
|
| Williamplasticity |
160 |
160 |
| Ukuqina (ShoreA) |
43 |
43 |
| Ukuminyana(g/cm3) | 1.125 |
1.14 |
| Amandla e-Tensile (MPa) |
10.0 |
10.0 |
| Ubude(%) | 700 |
700 |
| Amandla wezinyembezi (kN/m) | 25 |
25 |
| I-Dielectric njalo ku-100HZ |
3.03 |
3.03 |
| Isici sokulahla ku-100HZ |
0.0029 |
0.0029 |
| Ukulandelela ukumelana | -- |
1A3.5 |
| Amandla e-Dielectric (kV/mm) | 24.3 |
24.3 |
| Ukungazweli Ivolumu (Ω·cm) | 1.0*1016 |
1.0*1016 |