GA-9442
Herchy
| Kuboneka: | |
|---|---|
| Umubare: | |
Ikizamini: DBPMH, gukiza bwa mbere: 170 ° C x 10min, gukiza post.200 ° C x4H.
| Ibipimo byibicuruzwa | ||
| Ibicuruzwa | GA-9442 |
GA-9443 |
| Kugaragara | umuhondo ucye |
|
| Yamamoto |
160 |
160 |
| Gukomera (ShoreA) |
43 |
43 |
| Ubucucike (g / cm3) | 1.125 |
1.14 |
| Imbaraga zingana (MPa) |
10.0 |
10.0 |
| Kurambura (%) | 700 |
700 |
| Amarira amarira (kN / m) | 25 |
25 |
| Dielectric ihoraho kuri 100HZ |
3.03 |
3.03 |
| Impamvu yo gutandukana kuri 100HZ |
0.0029 |
0.0029 |
| Gukurikirana ibiturwanya | - |
1A3.5 |
| Imbaraga za dielectric (kV / mm) | 24.3 |
24.3 |
| Ingano yo Kurwanya (Ω · cm) | 1.0 * 1016 |
1.0 * 1016 |