GA-9442
Herchy nga bwe kiri
| Ebiriwo: | |
|---|---|
| Omuwendo: | |
Okugezesa: DBPMH, okusooka okuwonya: 170°C x 10min, oluvannyuma lw’okuwonya.200°C x4H.
| Ebipimo by’ebintu ebikolebwa | ||
| Ekyamaguzi | GA-9442 |
GA-9443 |
| Endabika | kya kyenvu ekizibu |
|
| Obuveera bwa William |
160 |
160 |
| Obukaluba (ShoreA) . |
43 |
43 |
| Obugumu(g/cm3) . | 1.125 |
1.14 |
| Amaanyi g’okusika (MPa) . |
10.0 |
10.0 |
| Okuwanvuwa(%) . | 700 |
700 |
| Amaanyi g’okukutuka (kN/m) . | 25 |
25 |
| Ekikyukakyuka kya dielectric ku 100HZ |
3.03 |
3.03 |
| Ensonga y’okusaasaanya ku 100HZ |
0.0029 |
0.0029 |
| Okulondoola okuziyiza | -- |
1A3.5 |
| Amaanyi g’amasannyalaze (kV/mm) . | 24.3 |
24.3 |
| Obuziyiza bw’obuzito (Ω·cm) . | 1.0*1016 |
1.0*1016 |