GA-9442
Herchy
| Disponibilite: | |
|---|---|
| Kantite: | |
Tès: DBPMH, premye geri: 170°C x 10min, post curing.200°C x4H.
| Paramèt pwodwi | ||
| Pwodwi | GA-9442 |
GA-9443 |
| Aparans | endispoze jòn |
|
| Williamplasticity |
160 |
160 |
| Dite (ShoreA) |
43 |
43 |
| Dansite (g/cm3) | 1.125 |
1.14 |
| Fòs rupture (MPa) |
10.0 |
10.0 |
| elongasyon (%) | 700 |
700 |
| Fòs chire (kN/m) | 25 |
25 |
| Dielectric konstan nan 100HZ |
3.03 |
3.03 |
| Faktè dissipation nan 100HZ |
0.0029 |
0.0029 |
| Suivi rezistans | -- |
1A3.5 |
| Dyelèktrik fòs (kV/mm) | 24.3 |
24.3 |
| Rezistivite volim (Ω·cm) | 1.0 * 1016 |
1.0 * 1016 |