Teko: DBPMH, go fodiša la mathomo: 170 ° C x 10min, ka morago ga go fodiša.200 ° C x4H.
| Ditekanyetšo tša setšweletšwa | ||
| Setšweletšwa | GA - 9442 ya go tšhungwa |
GA-9443 ya go swana le yona |
| Ponagalo | mosehla o fokolang |
|
| Williamplasticity ya go dira dilo |
160 |
160 |
| Thata (LebopoA) . |
43 |
43 |
| Kitlano (g / cm3) . | 1.125 |
1.14 |
| Matla a go goga (MPa) . |
10.0 |
10.0 |
| Go telefatšwa(%) . | 700 |
700 |
| Matla a go gagola (kN/m) . | 25 |
25 |
| Dielectric kamehla ka 100HZ |
3.03 |
3.03 |
| Dissipation Ntlha ka 100HZ |
0.0029 |
0.0029 |
| Go latedisa go ganetša | -- . |
1A3.5 |
| Matla a Dielectric (kV / mm) . | 24.3 |
24.3 |
| Bophagamo bja go ganetša (Ω·cm) . | 1.0 * 10 e 10.016 |
1.0 * 10 e 10.016 |