GA-9442 Silicone rubber for cable accessories (DBPMH) (HCR)

Description Product: seri iki karet silikon tahan voltase dhuwur vulcanized dening DBPMH aplikasi Key: aksesoris kabel voltase penengah; terminal kontraksi kadhemen internal lan eksternal, sarung dll. 
Fitur utama: ngecor injeksi, tensile dhuwur, elongation dhuwur, kekuatan luh dhuwur, deformasi cilik; lulus otentikasi RoHS lan REACH.
  • GA-9442

  • Herchy

kasedhiyan:
Jumlah:

Test: DBPMH, curing pisanan: 170°C x 10min, post curing.200°C x4H.

Parameter produk
produk GA-9442
GA-9443
Penampilan kuning samar
Williamplastisitas
160
160
Kekerasan (ShoreA)
43
43
Kapadhetan (g/cm3) 1.125
1.14
Kekuatan tarik (MPa)

10.0
10.0
Elongasi (%) 700
700
Kekuwatan sobek (kN/m) 25
25
Konstanta dielektrik ing 100HZ
3.03

3.03

Faktor disipasi ing 100HZ
0.0029
0.0029
nelusuri resistance --
1A3.5
Kekuwatan Dielektrik (kV/mm) 24.3


24.3

Resistivitas Volume (Ω·cm) 1.0*1016
1.0*1016









Sadurunge: 
Sabanjure: 

LINKS CEPAT

PRODUK KAMI

INFORMASI KONTAK

Tambah: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Telpon / WhatsApp / Skype: +86 15221953351
Hak Cipta     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |   Kebijakan Privasi | Dhukungan dening Leadong.