GA-9442
Herchy
| Helitaanka: | |
|---|---|
| Tirada: | |
Tijaabada: DBPMH, daawaynta koowaad: 170°C x 10min, daawaynta ka dib.200°C x4H.
| Xuduudaha alaabta | ||
| Alaabta | GA-9442 |
GA-9443 |
| Muuqashada | huruud daciif ah |
|
| Williamplasticity |
160 |
160 |
| Adag ( ShoreA) |
43 |
43 |
| Cufnaanta (g/cm3) | 1.125 |
1.14 |
| Xoog xajin (MPa) |
10.0 |
10.0 |
| Dheeraynta(%) | 700 |
700 |
| Xoogga jeexjeexa (kN/m) | 25 |
25 |
| Dielectric joogto ah oo ah 100HZ |
3.03 |
3.03 |
| Qodobka kala daadsanaanta 100HZ |
0.0029 |
0.0029 |
| Iska caabinta raadraaca | -- |
1A3.5 |
| Xoogga Dielectric (kV/mm) | 24.3 |
24.3 |
| Cabbitaanka mugga (Ω·cm) | 1.0*1016 |
1.0*1016 |