GA-6071AHT
Herchy
| Kuwanikwa: | |
|---|---|
| Huwandu: | |
GA-6071AHT Silicone Rubber yeUltra-high Voltage Cable (HCR)
Chishandiso: chakakodzera kugadzira girinhi simba rakakwirira voltage yakadzivirirwa tambo, yakakwirira-inodzivirira tambo, njanji yekufambisa tambo, nezvimwe.
Zvinhu zvakakosha: inoenderana nezvinodiwa zve 1S06722-1: 2011 (E), GB/T33430-2016, uye LV 216; Yakanakisa yakakwirira uye yakaderera tembiricha kuramba, yakanaka extrusionprocessability, yakanaka magetsi ekudzivirira chivakwa; Paridza muyedzo wekuchembera kwekushisa kwe3000h uye DC system neCD.
Muedzo: platinum A: 0.3%, platinum B: 1.2%, 130 ℃ x 5min.
| CLASS E(180℃)Chigadzirwa paramita | |||
| Product | GA-6071AHT | GA-6071AHTAB | |
| Chitarisiko | Translucent | ||
| Williamplasticity | 265 | 265 | |
| Kuoma (ShoreA) | 65 | 68 | |
| Density(g/cm3) | 1.2 | 1.2 | |
| Tensile simba (MPa) | 10 | 10.5 | |
| Elongation(%) | 450 | 700 | |
| Simba rekubvarura (kN/m) | 33 | 45 | |
| Volume resistivity (Ω·cm) | 1.0*1015 | 1.0*1015 | |
| Kuputsa simba (kV/mm) | 25 | 25 | |