Application: ordinary buttons, seals and other conventional strength products. o Key features: good resilience, excellent processab小ty, pass the authentication of RoHS, REACH, and FDA.
Application: anti yellowing requirements of high-end buttons, sealing product etc. Key Features: good anti-yellowing property, high transparence, excellentprocessability, pass the authentication of RoHS, REACH, and FDA
Application: flame retardant miscellaneous for auto parts, heating belt of air conditioner,and flame retardant gasket, etc. Keyfeatures:high strength,halogen-free and sulfur-free flame retardant, pass the authentication of RoHS and REACH.
Application: suitable for producing all kinds of flame-retardant products. Key features: high strength, halogen-free flame「etardant,excellent flame retardancy,pass the authentication of RoHS and REACH.
Application: suitable for producing buttons, etc. Key features: high strength, high rebound resilience, the service life is up to 10 milliontimes, pass the authentication of RoHS, REACH, and FDA
Application: suitable for the production of gas phase extrusion products such as hose,sealing strip etc. Key features: good anti-yellowing property, excellent processab小ty,pass theauthentication of RoHS, REACH, and LFGB.