I-GA-81×2P irabha ye-silicone e-retardant flame enamandla amakhulu (HCR)
Uhlelo lokusebenza: i-flame retardant ingxubevange yezingxenye zezimoto, ibhande lokushisisa le-air conditioner, kanye ne-gasket retardant flame, njll.
Izici ezibalulekile:amandla aphezulu, i-halogen-free kanye ne-sulfur-free flame retardant, idlulisa ukuqinisekiswa kwe-RoHS kanye ne-REACH.