GA-97XX Oil Resistant Silicone Rubber (HCR)

GA-97XX Oil Resistant Silicone Rubber (HCR)
Application: suitable for the production of oil resistant products.
Key features: high strength, good tolerance with ASTM 1# and IRM903 Oil, pass theauthentication of RoHS and REACH.
 
  • GA-97XX

  • Herchy

Availability:
Quantity:

GA-97XX Oil Resistant Silicone Rubber (HCR)


Application: suitable for the production of oil resistant products.
Key features: high strength, good tolerance with ASTM 1# and IRM903 Oil, pass theauthentication of RoHS and REACH.
Test: 1% of curing agent (50% paste of DBPMH in silicone gum), 175°Cx5min x15MPa.



Product parameters
ProductGA-9740GA-9750GA-9760GA-9770
AppearanceGray
Williamplasticity140180200260
Hardness (ShoreA)40506070
Density(g/cm3)1.231.251.281.32
Tensile strength (MPa)3.54.555.5
Elongation(%)700600400250
Tear strength (kN/m)15151515
175"C x22h Compression(%)20202020
Air ageing 225°C x70HHardness change1222
Tension strength change rate-25%-25%-25%-25%
Rate of elongation change-30%-30%-30%-30%
IRM903oil 150°C x70HHardness change-18-18-17-16
Tension strength change rate-35%-35%-35%-35%
Rate of elongation change-20%-20%-20%-20%
Volume change36%36%35%35%


Previous: 
Next: 

QUICK LINKS

OUR PRODUCTS

CONTACT INFORMATION

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +8615221953351
Copyright  2023 Shanghai Herchy Rubber Co., Ltd. Sitemap |  Privacy Policy | Support By Leadong.