GA-97XX
Herchy
| Wāteatanga: | |
|---|---|
| Rahi: | |
GA-97XX Hinu Atete Silicone Rubber (HCR)
Taupānga: e tika ana mo te hanga o nga hua aukati hinu.
Ko nga ahuatanga matua: te kaha teitei, te pai o te manawanui me te ASTM 1 # me te hinu IRM903, tukuna te motuhēhēnga o te RoHS me te REACH.
Whakamatau: 1% o te kaihoko whakaora (50% te whakapiri o te DBPMH i roto i te kapia silicone), 175°Cx5min x15MPa.
| Tawhā hua | |||||
| Hua | GA-9740 | GA-9750 | GA-9760 | GA-9770 | |
| Te ahua | Kerei | ||||
| Williamplasticity | 140 | 180 | 200 | 260 | |
| Maama (ShoreA) | 40 | 50 | 60 | 70 | |
| Kiato(g/cm3) | 1.23 | 1.25 | 1.28 | 1.32 | |
| Te kaha o te kaha (MPa) | 3.5 | 4.5 | 5 | 5.5 | |
| Whakaroa(%) | 700 | 600 | 400 | 250 | |
| Te kaha roimata (kN/m) | 15 | 15 | 15 | 15 | |
| 175'C x22h Kōpeketanga(%) | 20 | 20 | 20 | 20 | |
| Hurihia te hau 225°C x70H | Te huringa pakeke | 1 | 2 | 2 | 2 |
| Rereke huringa kaha mānukanuka | -25% | -25% | -25% | -25% | |
| Te tere o te huringa whakaroa | -30% | -30% | -30% | -30% | |
| IRM903hinu 150°C x70H | Te huringa pakeke | -18 | -18 | -17 | -16 |
| Rereke huringa kaha mānukanuka | -35% | -35% | -35% | -35% | |
| Te tere o te huringa whakaroa | -20% | -20% | -20% | -20% | |
| Hurihia te rōrahi | 36% | 36% | 35% | 35% | |