GA-97XX Raba ya Silicone leyi nga ngheniwiki hi oyili (HCR) .
Xitirhisiwa: xi lulamerile eka vuhumelerisi bya switirhisiwa leswinga tiyela oyili.
Swihlawulekisi swa nkoka: matimba ya le henhla, ku tiyisela lokunene na ASTM 1 # na IRM903 Oil, ku hundza theauthentication ya RoHS na REACH.
Xikambelo: 1% wa xiaki xo horisa (50% wa paste ya DBPMH eka silicone gum), 175°Cx5min x15MPa.
| Tipharamitha ta Xiendliwa . | |||||
| Ximakiwa | GA-9740 | GA-9750 | GA-9760 | GA-9770 | |
| Xivumbeko | Mpunga | ||||
| WilliamPlasticity . | 140 | 180 | 200 | 260 | |
| Ku nonon'hwa (Shorea) . | 40 | 50 | 60 | 70 | |
| Ku tsindziyela(g/cm3) . | 1.23 | 1.25 | 1.28 | 1.32 | |
| Matimba ya ku tsana (MPA) . | 3.5 | 4.5 | 5 | 5.5 | |
| Ku leha(%) . | 700 | 600 | 400 | 250 | |
| Matimba yo handzula (kN/m) . | 15 | 15 | 15 | 15 | |
| 175'C x22h Ntshikelelo(%) | 20 | 20 | 20 | 20 | |
| Ku dyuhala ka moya 225°C x70H | Ku cinca ka ku tiya | 1 | 2 | 2 | 2 |
| Nhlayo ya ku cinca ka matimba ya tension | -25% . | -25% . | -25% . | -25% . | |
| Mpimo wa ku cinca ka ku leha | -30% . | -30% . | -30% . | -30% . | |
| IRM903oyili ya 150°C x70H | Ku cinca ka ku tiya | -18 | -18 | -17 | -16 |
| Nhlayo ya ku cinca ka matimba ya tension | -35% . | -35% . | -35% . | -35% . | |
| Mpimo wa ku cinca ka ku leha | -20% . | -20% . | -20% . | -20% . | |
| Ku cinca ka vholumo | 36% . | 36% . | 35% . | 35% . | |