GA-97XX Omupiira oguziyiza amafuta ga silikoni (HCR)

GA-97XX Omupiira oguziyiza amafuta ga silikoni (HCR)
Okukozesa: kirungi okukola ebintu ebigumira amafuta.
Ebikulu: amaanyi amangi, okugumiikiriza okulungi ne ASTM 1 # ne IRM903 Oil, okuyita theauthentication ya RoHS ne REACH.
 
  • GA-97XX

  • Herchy nga bwe kiri

Okubeerawo:
Omuwendo:

GA-97XX Omupiira oguziyiza amafuta ga silikoni (HCR)


Okukozesa: kirungi okukola ebintu ebigumira amafuta.
Ebikulu: amaanyi amangi, okugumiikiriza okulungi ne ASTM 1 # ne IRM903 Oil, okuyita theauthentication ya RoHS ne REACH.
Okugezesa: 1% eky’ekirungo ekiwonya (50% ekikuta kya DBPMH mu silicone gum), 175°Cx5min x15MPa.



Ebipimo by’ebintu
Ekyamaguzi GA-9740 GA-9750 GA-9760 GA-9770
Endabika Gray
Obuveera bwa William 140 180 200 260
Obukaluba (ShoreA) . 40 50 60 70
Obugumu(g/cm3) . 1.23 1.25 1.28 1.32
Amaanyi g’okusika (MPA) . 3.5 4.5 5 5.5
okuwanvuwa(%) . 700 600 400 250
Amaanyi g’okukutuka (kN/m) . 15 15 15 15
175'C x22h Okunyigiriza(%) 20 20 20 20
Empewo ekaddiwa 225°C x70H Enkyukakyuka y’obukaluba 1 2 2 2
Enkyukakyuka y’amaanyi g’okusika omuguwa -25% -25% -25% -25%
Omutindo gw’enkyukakyuka mu kuwanvuwa -30% -30% -30% -30%
IRM903amafuta 150°C x70H Enkyukakyuka y’obukaluba -18 -18 -17 -16
Enkyukakyuka y’amaanyi g’okusika omuguwa -35% -35% -35% -35%
Omutindo gw’enkyukakyuka mu kuwanvuwa -20% -20% -20% -20%
Enkyukakyuka mu ddoboozi 36% 36% Ebitundu 35% Ebitundu 35%


Jjuuzi: 
Ekiddako: 

ENKOZESA Y'AMAWANGA

EBINTU EBYAFFE

AMAWULIRE AG'OKUKWATAGANA

Gattako: No.33, Lane 159, oluguudo lwa Taiye, mu Disitulikiti y’e Fengxian, Shanghai
Essimu / WhatsApp / Skype ku ssimu: +86 15221953351
Eddembe ly’okuwandiika     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap y'ekifo |   Enkola y'Ebyama | Obuwagizi Bwa... Leadong.