Rubber green strength tihchangtlun dan tur

Tire siam chhuah stage hnihnaah rupture venna kawngah emaw, gravitational force avanga complex extruded profile a tlakchhiat loh nan emaw green strength hi a rit hle a ni.

1. Molecular weight-in nghawng a neih dan

A tlangpuiin, elastomer thlan molecular weight a san chuan Green-a chakna a sang zawk thin. SBR-ah chuan average molecular weight sang tak hman a ni a, mahse molecular weight sang lutuk chuan processing lama harsatna dang a thlen thei a ni.

2. Strain hmanga crystallisation tihchhuah

Strain-induced crystallisation nei adhesives te hian Green’s strength sang tak an nei tlangpui.

3. Natural rubber hmanga siam a ni

Natural rubber hian Green’s strength a nei sang hle. NR hian Green’s strength sang tak a nei a, a chhan chu a stretch chuan a crystallise thin. Natural glue-ah hian fatty acid ester group tam zawk a awm a, hei hi tension-a crystallisation a tam zawk avangin Green-a chakna a sang zawk a, a tlangpuiin fatty acid ester group awm zat tlem ber chu 2.8 mmol/kg vel a ni.

4. Polymer te block thin

Random copolymer SBR adhesives-a block styrene tlemte awm hian adhesive hi Green-a chakna tha tak a pe thei a ni.

5. Semi-crystalline EPDM hmanga siam a ni

Ethylene tamna semi-crystalline EPDM thlan hian room temperature-ah adhesive chu Green’s strength tha tak a pe thei a ni.

6. Metallocene hmanga tihchak EPDM

Single active center limited geometry metallocene catalyst technology hmang hian ethylene tamna EPDM chu nasa takin siam chhuah theih a ni. He EPDM ethylene tamna hian Green’s strength sang tak a nei a ni. He technology hmang hian ethylene awm zat chu tihdanglam theih a ni a, Green-a EPDM chakna pawh a tipung lehzual thei bawk.

7. Molecular weight insem dan

NBR compound molecular weight distribution tawi tak nei te hian Green’s strength sang tak an nei a.

8. CR

High Green chakna hi fast crystallising neoprene thlan atanga hmuh theih a ni. CR-a styrene tamna SBR dah belh hian Green chakna a ti sang thei a ni.

Neoprene chi hrang hrang zingah hian Type T neoprene hian collapse leh deformation do theihna tha ber a nei a, chu chu Green’s strength sang ber a ni a, a dawttu chu Type W. Type G neoprene hian Green’s strength a nei chhe ber a ni.

9. Polytetrafluoroethylene hmanga siam a ni

Teflon additives hian Green-a adhesive chakna a tichak a.

10. Carbon dum a ni

Carbon black hian surface area sang tak leh structure sang tak a nei a, Green hian rubber chakna a ti sang hle. n326 hi tire wire covering-ah hman fo a ni a, a chhan chu rubber chu Green’s strength sang tak a pe a, chutih rualin wire luh theihna tur viscosity a hniam tawk bawk.

Green’s strength tha tak neih nan chuan carbon black structure sang tak leh specific surface area hniam tak hman tur a ni. Hei hi a chhan chu specific area hniam carbon black hian filling volume sang zawk a phal a, chu chuan Green chakna a tipung a ni.

11. Mixing

Mixing process-ah hian elastomer chu over-plasticized a nih chuan Green-a compound chakna chu a tlahniam ang.

QUICK LINKS A AWM VE ANG

CONTACT THIL AWM DAN

Add: No.33, Lane 159, Taiye kawngpui, Fengxian District, Shanghai-a awm a ni
Tel / WhatsApp / Skype: +86 15221953351 ah zawhfiah theih a ni
E-mail hmangin:  info@herchyrubber.com
A rilru a hah   lutuk chuan a rilru   2023 a buai em em a. Shanghai Herchy Rubber Co., Ltd. Sitemap a ni |   Thuruk humhalh dan tur | Support By Leadong a ni.