Ike akwụkwọ ndụ akwụkwọ ndụ dị oke ibu ma a bịa n'ịgbochi mgbawa n'oge ọkwa nke abụọ nke mmepụta taya ma ọ bụ mgbe ọ na-abịa igbochi ọdịda nke profaịlụ extruded dị mgbagwoju anya n'ihi ike ndọda.
1. Mmetụta nke ịdị arọ molekụla
N'ikwu okwu n'ozuzu, ka ịdị arọ nke elastomer na-ahọrọ dị elu, ka ike Green na-adị elu. N'ihe banyere SBR, a na-eji ịdị arọ dị elu nke dị elu mee ihe, ma ịdị arọ nke molekụla dị elu nwere ike ịkpata nsogbu nhazi ndị ọzọ.
2. kristal na-akpata nsogbu
Adhesives nwere kristal na-akpata nsogbu na-enwekarị ike Green dị elu.
3. Eke roba
Eke roba nwere ike Green dị elu. NR nwere ike Green dị elu n'ihi na ọ na-egbuke egbuke mgbe agbatị. Gluo ndị sitere n'okike nwere ọdịnaya dị elu nke fatty acid ester otu nwere ike Green dị elu n'ihi ogo kristal dị ukwuu na esemokwu, n'ozuzu ya nwere obere ọdịnaya nke otu ester fatty acid dị ihe dị ka 2.8 mmol/kg.
4. Block polymers
Ọnụnọ nke obere ihe mgbochi styrene na nrapado copolymer SBR nwere ike inye nrapado ahụ ezigbo ike Green.
5. Semi-kristal EPDM
Nhọrọ nke semi-crystalline EPDM nwere ọdịnaya ethylene dị elu nwere ike inye ihe nrapado ahụ ezigbo ike Green na okpomọkụ ụlọ.
6. Metallocene-catalyzed EPDM
Otu ụlọ ọrụ na-arụ ọrụ nwere obere teknụzụ geometry metallocene na-enyere aka imepụta ọdịnaya EPDM dị elu n'ọtụtụ buru ibu. EPDM a nwere ọdịnaya ethylene dị elu nwere ike Green dị elu. Site na teknụzụ a enwere ike ịhazi ọdịnaya ethylene yana ike Green nke EPDM ga-abawanye.
7. Nkesa arọ molecular
Ngwakọta NBR nwere nkesa arọ molekụla dị warara nwere ike Green dị elu.
8. CR
Enwere ike nweta ike Green dị elu site na ịhọrọ neoprene na-egbuke egbuke. Mgbakwunye SBR nwere ọdịnaya styrene dị elu na CR nwere ike melite ike Green.
N'ime ụdị dị iche iche nke neoprene, Ụdị T neoprene nwere nkwụsị kachasị mma nke ịdaba na nrụrụ, ya bụ ike Green kachasị elu, na-esote Ụdị W. Ụdị G neoprene nwere ike Green kasị njọ.
9. Polytetrafluoroethylene
Ihe mgbakwunye Teflon na-eme ka ike Green nke nrapado dịkwuo mma.
10. Carbon ojii
Carbon ojii nwere oke elu na ihe owuwu dị elu na-eme ka ike Green nke rọba dịkwuo mma. A na-ejikarị n326 eme ihe na mkpuchi taya taya n'ihi na ọ na-enye rọba ike Green dị elu ma na-eme ka viscosity dị ala nke ọma maka waya ịbanye.
Maka ike Green dị mma, a ga-eji carbon ojii nwere usoro dị elu na ebe dị elu dị ala. Nke a bụ n'ihi na obere mpaghara carbon ojii na-enye ohere maka oke njuputa dị elu, nke na-eme ka ike Green dịkwuo elu.
11. Ngwakọta
N'ime usoro ngwakọta, ọ bụrụ na elastomer na-ekpuchi elu-plastic, ike Green nke ogige ga-ebelata.