FV9200
Herchy
| Ri fhaotainn: | |
|---|---|
| Meud: | |
Nithean |
Comharran |
|||
Ìrean |
FV9240 |
FV9250 |
FV9260 |
|
Dòighean Deuchainn / Coltas |
Milky geal tar-shoilleir |
|||
Gravity sònraichte / g / cm3 |
ASTM D792 |
1.42 |
1.44 |
1.45 |
cruas/cladach A |
ASTM D2240 |
40 |
50 |
60 |
Neart tensile/MPa |
ASTM D412 |
10.1 |
10.2 |
10.3 |
Meudachadh aig briseadh / % |
ASTM D412 |
490 |
457 |
440 |
Neart deòir/KN/m |
ASTM D624-B |
35 |
42 |
43 |
Seata teannachaidh (177 ℃ * 22h) |
ASTM D395 |
11 |
11 |
12 |
* Seasmhachd teas |
Atharrachadh cruas / cladach A |
+3 |
+3 |
+2 |
Atharrachadh neart tensile, % |
-19 |
-16 |
-17 |
|
Leudachadh aig atharrachadh briseadh, % |
-14 |
-17 |
-18 |
|
connadh C Atharrachadh fuaim/% 23 ℃ / 72 h |
ASTM D471 |
23 |
21 |
20 |
Suidheachadh leigheas |
0.7 DBPH, Press leigheas: 170 ℃ × 15min , Post leigheas: 200 ℃ × 4h |
|||
Gnìomhan a thathar a’ moladh:
Thathas a’ moladh pàirt 0.6 gu 1 de àidseant ceimigeach bisdipenta a chleachdadh airson vulcanization (2,5-dimethyl-2,5-bis (tert-butylperoxy) hexane).
Bu chòir do luchd-ceannach an teòthachd agus an ùine as freagarraiche a thaghadh airson leigheas a rèir meud an toraidh agus an dòigh ciùraigidh.
Pacadh toraidh:
Chan eil an toradh seo cunnartach, an àite sin tha e air a dhèanamh suas de stoc cairt, plastaig, agus 10 cileagram gach poca, 2 phoca gach bogsa.
Aois stòraidh:
Tha comas sruthadh fuar aig an toradh seo, bu chòir am baga a sheachnadh gus nach tèid a mhilleadh aig àm còmhdhail no cleachdadh.
Cùm ann an àrainneachd fionnar, tioram le beatha sgeilp de 12 mìosan.