GA-93X0 Silikoni ka lastikuw (silica précipitation)(HCR) .

A kɛcogo: A bɛnnen don ka sigilan sirilan ni fɛn wɛrɛw dilan.
Fɛn min ye fɛnba ye: Tumu joli ɲuman, tulu hakɛ bɛ tɛmɛ 7% kan, tɛmɛ ROHS ni REACH.
  • GA-93X0 .

  • Herchy .

Sɔrɔli:
Hakɛ:

Kɔrɔbɔli: 1% furakɛli fura (50% DBPMH INS小Conegum),175°C x 5min x 15MPa.


Product Paramɛtɛrɛw .
Ka kɛ GA-9330 . GA-9340 . GA-9350 . GA-9360 . GA-9370 .
Yecogo Nɔnɔw bɛ min na .
WilliamPlasticity . 140 170 200 220 240
Gɛlɛya (Shoaa) . 30 40 50 60 70
density(G/CM3) . 1.12 1.14 1.17 1.2 1.21
Tensile fanga (MPa) . 9 10 10 8.5 8.5
elongation(%) . 850 800 700 500 350
Ɲɛjibɔ fanga (KN/M) . 20 25 30 25 25


Tɛmɛnen: 
Nata: 

Link teliyalenw .

An ka fɛn dilannenw .

Kunnafoni minnu bɛ sɔrɔ .

Fàra o kan: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Sitemap . |   Kunnafoni-falen-falen sariyaw | dɛmɛ don ni . Leadong ..