GA-93x0 Sels smeerende silikonbrub (Dingen presipeare silica) (HCR)

Oanfraach: Geskikt foar produksje fan sealingstekker en oare produkten.
Key Funksje: Goede oalje-blijdende eigendom, de oaljele ynhâld is mear dan 7%, pas teautykjen fan Rohs en berik.
  • GA-93X0

  • Herchy

Beskikberens:
kwantiteit:

TOST: 1% fan genêzen agint (50% pasta fan DBPMH Ins 小 Conegum), 175 ° C x 5min x 15mpa.


Produktparameters
Produkt GA-9330 GA-9340 GA-9350 GA-9360 GA-9370
Ferskining MilkyWhite
Williamplasticity 140 170 200 220 240
Hurdens (Shorea) 30 40 50 60 70
DENSITY (G / CM3) 1.12 1.14 1.17 1.2 1.21
Tensile krêft (MPA) 9 10 10 8.5 8.5
ELONGATION (%) 850 800 700 500 350
Slachterkast (KN / M) 20 25 30 25 25


Foarige: 
Folgjende: 

Fluchkeamers

Ús produkten

KONTAKT YNFORMAASJE

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai herchy rubber Co., Ltd. Sitemap |   Privacybelied | Stypje troch Leadong.