GA-93X0 Self-Lubricating Rubber Silicone (Silica Precipitated) (hcr)

Serlêdan: Ji bo hilberîna pêveka sekinandina plug û hilberên din.
Taybetmendiya KEY: Taybetmendiya rûnê ya rûnê ya rûnê, naveroka neftê ji% 7 e, Theauthentation of Rohs û gihîştî derbas bikin.
  • Ga-93x0

  • Herchy

Hatility:
Qumar:

Test: 1% ji Agent Curing (50% Paste of DBPMH Ins 小 Conegum), 175 ° C X 5min X 15mpa.


Parametreyên hilberê
Mal GA-9330 GA-9340 GA-9350 GA-9360 GA-9370
Xuyabûnî MilkyWhite
Williamplasticity 140 170 200 220 240
Hardness (Shorea) 30 40 50 60 70
Dendik (g / cm3) 1.12 1.14 1.17 1.2 1.21
Hêza Tensile (MPa) 9 10 10 8.5 8.5
Elongation (%) 850 800 700 500 350
Hêza tirşikê (kn / m) 20 25 30 25 25


Pêşî: 
Piştî: 

Zencîreyên Zûtir

Berhemên me

Agahdariya têkiliyê

Zêde: No.33, Lane 159, Taiye Road, District Fengxian, Shanghai
Tel / WhatsApp / Skype: +86 15221953351
Copyright     2023 Shanghai Herchy Rubber Co., Ltd. Nexşe |   Siyaseta Rizgarî | Piştgirî ji hêla Ledong.