ꯖꯤ.ꯑꯦ.-꯹꯳ꯑꯦꯛꯁ꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫
ꯍꯔꯆꯤ꯫
| ꯐꯪꯒꯗꯕꯥ: | |
|---|---|
| ꯃꯁꯤꯡ: ꯱. | |
ꯇꯦꯁ꯭ꯠ: ꯀ꯭ꯌꯨꯔꯤꯡ ꯑꯦꯖꯦꯟꯇꯀꯤ 1% (DBPMH ꯏꯅꯁ小ꯀꯣꯅꯦꯒꯃꯒꯤ 50% ꯄꯦꯁ꯭ꯠ),175°C x 5min x 15MPa.
| ꯄ꯭ꯔꯗꯛꯇ ꯄꯦꯔꯥꯃꯤꯇꯔꯁꯤꯡ꯫ | |||||
| ꯄꯣꯠꯊꯣꯛ | ꯖꯤ.ꯑꯦ.-꯹꯳꯳꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯳꯴꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯳꯵꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯳꯶꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ | ꯖꯤ.ꯑꯦ.-꯹꯳꯷꯰ꯗꯥ ꯌꯥꯑꯣꯔꯤ꯫ |
| ꯃꯄꯥꯟꯊꯣꯡꯗ ꯎꯕ | ꯃꯤꯜꯀꯤꯍꯣꯏꯠ꯫ | ||||
| ꯎꯏꯂꯤꯌꯥꯃꯞꯂꯥꯁ꯭ꯇꯤꯁꯤꯇꯤ ꯂꯩꯕꯥ꯫ | 140 | 170 | 200 | 220 | 240 |
| ꯍꯥꯔꯗꯅꯦꯁ (ꯁꯣꯔꯑꯦ) ꯑꯃꯁꯨꯡ ꯑꯦꯟ. | 30 | 40 | 50 | 60 | 70 |
| ꯗꯦꯟꯁꯤꯇꯤ(ꯖꯤ/ꯁꯦ.ꯃꯤ.꯳) ꯑꯁꯤꯅꯤ꯫ | 1.12 | 1.14 | 1.17 | 1.2 | 1.21 |
| ꯇꯦꯟꯁꯥꯏꯜ ꯁ꯭ꯠꯔꯦꯡꯊ (ꯑꯦꯝ.ꯄꯤ.ꯑꯦ.) ꯑꯃꯁꯨꯡ ꯑꯦꯝ.ꯄꯤ.ꯑꯦ. | 9 | 10 | 10 | 8.5 | 8.5 |
| ꯏꯂꯣꯡꯒꯦꯁꯟ(%) ꯴. | 850 | 800 | 700 | 500 | 350 |
| ꯇꯤꯌꯥꯔ ꯁ꯭ꯠꯔꯦꯡꯊ (kN/m) ꯑꯁꯤꯅꯤ꯫ | 20 | 25 | 30 | 25 | 25 |