Qormaata: %1 kan fayyisu (%50 paastaa DBPMH ins小conegum),175°C x 5min x 15MPa.
| Parameetaroota oomishaa | |||||
| Oomisha | GA-9330 irratti kan argamu | GA-9340 irratti kan argamu | GA-9350 irratti kan argamu | GA-9360 irratti kan argamu | GA-9370 irratti kan argamu |
| Mul'ina | MilkiiAdii | ||||
| Wiliyaampilaastikii | 140 | 170 | 200 | 220 | 240 |
| Jabina (ShoreA) . | 30 | 40 | 50 | 60 | 70 |
| Dandeettii(g/cm3) . | 1.12 | 1.14 | 1.17 | 1.2 | 1.21 |
| Jabina harkisaa (MPa) . | 9 | 10 | 10 | 8.5 | 8.5 |
| Dheersuu(%) . | 850 | 800 | 700 | 500 | 350 |
| Jabina ciccituu (kN/m) . | 20 | 25 | 30 | 25 | 25 |