S537-3
SK
EPDM
| Availability: | |
|---|---|
| Quantity: | |
【low ENB heat resistance Tire ethylene propylene rubber-EPDMS537-3】
Product Description
Low ENB heat resistance Tire ethylene propylene rubber-EPDM S537-3 is a kind of advanced rubber material with low ENB content and excellent heat resistance. It has good fluidity, good processability, low Mooney and good resistance to ozone. It is widely used in tire inner tube field and other rubber products.
Product Characteristics
(1) Low ENB Content: EPDM S537-3 has low ENB content, which can improve the physical properties of rubber products and reduce the cost of raw materials.
(2) Excellent Heat Resistance: EPDM S537-3 has excellent heat resistance, which can withstand high temperatures and maintain good physical properties.
(3) Good Fluidity and Processability: EPDM S537-3 has good fluidity and processability, which can improve the processing efficiency and reduce the processing cost.
(4) Low Mooney: EPDM S537-3 has low Mooney, which can reduce the processing cost and improve the processing efficiency.
(5) Good Resistance to Ozone: EPDM S537-3 has good resistance to ozone, which can withstand the test of ozone and maintain good physical properties.
Application
EPDM S537-3 is widely used in tire inner tube and other rubber products in the fields of automobiles, construction, shipbuilding, electronic appliances, cables, sealing and other industries. It is a very promising rubber material.