Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 5.7%
Ethylene content: 58%
Mooney viscosity: ML(1+4)125°C 84
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 4.1%
Ethylene content: 53%
Mooney viscosity: ML(1+4)125°C 30
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 5.5%
Ethylene content: 68%
Mooney viscosity: ML(1+4)125°C 87
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 5.7%
Ethylene content: 71%
Mooney viscosity: ML(1+4)125°C 24
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 6.5%
Ethylene content: 68%
Mooney viscosity: ML(1+4)125°C 135
Size: 25kg/block
MOQ: 25kg
Packing: boxed