Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.7%
Ethylene Nilalaman: 60%
Nilalaman ng langis: 75%
Mooney Viscosity: ML (1+4) 125 ° C 50
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 2.3%
Ethylene Nilalaman: 57%
Mooney Viscosity: ML (1+4) 125 ° C 35
Sukat: 25kg/Block
MOQ: 25kg
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 5.0%
nilalaman ng etilena: 64%
nilalaman ng langis : 75%
viscosity ng mooney: ml (1+4) 125 ° C 55
Sukat: 25kg/block
moq: 25kg
packing: boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.5%
Ethylene Nilalaman: 69%
Mooney Viscosity: ML (1+4) 125 ° C 63
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.7%
Ethylene Nilalaman: 70%
Nilalaman ng langis : 75%
Mooney Viscosity: ML (1+4) 125 ° C 62
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 1.0%
nilalaman ng ethylene: 66%
Mooney Viscosity: ML (1+4) 125 ° C 46
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed