Tlase ENB Heat Resistance Tyre Ethylene Propylene Rubber-EPDM
Ponahalo le boemo: bosoeu (bo bonaletsang kapa bo feto-fetohang) blocky
Mofuta oa boraro oa monomer le litaba: ENB, 2.3%
Likahare tsa ethylene: 57% Likahare tsa ethylene: 57%
Mooney viscosity: ML (NB, 2.3% Mooney viscosity: ML (1+4) 125 ° C 35
Boholo: 25kg / thibela
MOQ: 25kg