Appearance and condition: Beige or pale yellow blocky
Third monomer type and content: ENB, 4.4%
Ethylene content: 68.6%
Mooney viscosity: ML(1+4)125°C 77
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: Beige or pale yellow blocky
Third monomer type and content: ENB, 8.9%
Ethylene content: 60.1%
Mooney viscosity: ML(1+4)100°C 64
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 4.1%
Ethylene content: 58%
Mooney viscosity: ML(1+4)125°C 84
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Appearance and condition: white (transparent or translucent) blocky
Third monomer type and content: ENB, 4.7%
Ethylene content: 70%
Oil content:75%
Mooney viscosity: ML(1+4)125°C 62
Size: 25kg/block
MOQ: 25kg
Packing: boxed