Rezistans dlo Aparèy nan kay Ethylene Propylene Rubber-EPR
Aparans ak kondisyon: blan (transparan oswa translusid) blocky
Twazyèm kalite monomère ak kontni: ENB, 4.7%
kontni Ethylene: 60%
kontni lwil oliv: 75%
viskozite Mooney: ML (1 + 4) 125 ° C 50
Size: 25kg / blòk
MOQ: 25kg
anbalaj: bwat