Hitsura at kundisyon: Beige o maputlang dilaw na blocky
Pangatlong uri ng monomer at nilalaman: ENB, 8.9%
Ethylene content: 60.1%
Mooney viscosity: ML(1+4)100°C 64
Size: 25kg/block
MOQ: 25kg
Packing: boxed
Hitsura at kundisyon: Beige o maputlang dilaw na blocky
Ikatlong uri ng monomer at nilalaman: ENB, 4.4%
Ethylene content: 68.6%
Mooney viscosity: ML(1+4)125°C 77
Size: 25kg/block
MOQ: 25kg
Packing: boxed