Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 4.7% Ethylene content: 70% Oil content:75% Mooney viscosity: ML(1+4)125°C 62 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 9.4% Ethylene content: 55% Mooney viscosity: ML(1+4)125°C 29 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 5.7% Ethylene content: 58% Mooney viscosity: ML(1+4)125°C 84 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 8.5% Ethylene content: 72% Oil content:100% Mooney viscosity: ML(1+4)125°C 47 Size: 25kg/block MOQ: 25kg Packing: boxed
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 2.3% Ethylene content: 57% Mooney viscosity: ML(1+4)125°C 35 Size: 25kg/block MOQ: 25kg
Appearance and condition: white (transparent or translucent) blocky Third monomer type and content: ENB, 5.5% Ethylene content: 68% Mooney viscosity: ML(1+4)125°C 87 Size: 25kg/block MOQ: 25kg Packing: boxed