Mooney Low Ethylene Cable Ethylene Propylene Rubber-EPDM
Muuqashada iyo xaaladda: caddaan (daah-furan ama hufan) xannibaad
Nooca monomerka saddexaad iyo waxa ku jira: ENB, 5.7%
Ethylene content: 71%
Mooney viscosity: ML(1+4)125°C 24
Cabbir: 25kg/block
MOQ: 25kg
Xidhmada: sanduuqed