Hitsura at kondisyon: beige o maputlang dilaw na blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.5%
nilalaman ng etilena: 55.5%
lagkit ng mooney: ml (1+4) 125 ° C 55
Sukat: 25kg/block
moq: 25kg
packing: boxed
Hitsura at kondisyon: beige o maputlang dilaw na blocky
pangatlong uri ng monomer at nilalaman: ENB, 8%
nilalaman ng etilena: 60%
viscosity ng mooney: ml (1+4) 125 ° C 43
nilalaman ng langis: 100%
laki: 25kg/block
moq: 25kg
packing: boxed
Hitsura at kondisyon: beige o maputlang dilaw na blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.7%
nilalaman ng etilena: 68.3%
Mooney Viscosity: ML (1+4) 125 ° C 28
Nilalaman ng langis: 43%
Laki: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.7%
Ethylene Nilalaman: 60%
Nilalaman ng langis: 75%
Mooney Viscosity: ML (1+4) 125 ° C 50
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
pangatlong uri ng monomer at nilalaman: ENB, 4.1%
Ethylene Nilalaman: 58%
Mooney Viscosity: ML (1+4) 125 ° C 84
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed
Hitsura at kondisyon: puti (transparent o translucent) blocky
third monomer type at nilalaman: ENB, 4.1%
Ethylene Nilalaman: 53%
Mooney Viscosity: ML (1+4) 125 ° C 30
Sukat: 25kg/Block
MOQ: 25kg
Packing: Boxed