GA-91X1 Raba ya Silicone ya Antistatic (Silica leyi khulukaka) (HCR) .

Eka Shanghai Herchy Rubber Co., Ltd., hi nyika switirhisiwa swa rhaba ya xiyimo xa le henhla ya xiyimo xa le henhla (HCR) leswi hetisekeke eka tiindasitiri leti lavaka matirhelo ya le henhla na ku tshembheka. Xiendliwa xa hina xa GA-91X1 xi hlanganisa swivumbeko swa xiyimo xa le henhla swa antistatic, xi nyika nsirhelelo wo hlawuleka eka ku humesiwa ka electrostatic. Hiku engeteriwa ka silica leyi khulukaka, rhaba yi hlayisa swivumbeko swa kahle swinene swa michini, kukatsa na matimba yale henhla ya tensile xikan’we naku tiyisela. Kunga khathariseki leswaku u lava switirhisiwa swa switirhisiwa swa elektroniki, swisirhelelo, kumbe swiphemu swin’wana swa vukheta, hi tiyisisa leswaku xiendliwa xin’wana na xin’wana xi fikelela swipimelo swa indasitiri naswona xi endleriwe swilaveko swa wena swo karhi.
  • GA-91X1

  • Herchy

Ku kumeka:
Nhlayo: .

Ku nghenisiwa ka Raba ya hina ya GA-91X1 Antistatic Silicone (HCR) .


GA-91X1 Antistatic Silicone Rubber (HCR) leyingana precipitated silica i xitirhisiwa xa xiyimo xale henhla lexi endleriweke ku tiya swinene eka gezi xikan’we naku tiya hi michini. Raba leyi ya high-consistency (HCR) yi endleriwe switirhisiwa swa ti indasitiri leswi lavaka ku tiya ka le hansi ka le henhla na ku hangalaka ka static.


Nxaxamelo lowu wa rhaba ya silicone wunyika matirhelo yale henhla eka tindzhawu laha ku lawula electrostatic discharge (ESD) swinga swa nkoka. Yi hetisekile eka switirhisiwa eka swa elektroniki, vumaki, na tiindasitiri tin’wana leti lavaka switirhisiwa leswi nga cinciki.


Nxaxamelo wa GA-91X1 wu katsa tinxaka to tala leti nga na swiyimo swo hambana swa ku tiya, leswi endlaka leswaku yi cinciwa swinene ku fikelela swilaveko swa wena swo karhi swa matirhelo. Kunga khathariseki leswaku u lava ku tiyisela ka le henhla kumbe ku cinca-cinca loku antswisiweke, xiendliwa lexi xi nga lulamisiwa ku fambisana na swilaveko swa wena swa xikombelo.


Swihlawulekisi swo hlawuleka swa rhaba leyi swikatsa matimba yo tiya ya michini, ku olova swinene, na ku tiya lokukulu eka ku onhaka. Ku languteka ka translucent swinyika ku vonakala ko antswa, leswi kunga vuyelo bya nkoka eka tindzhawu tohambana hambana ta ti indasitiri.


Xikambelo: 1% wa xiaki xo horisa (50% wa paste ya DBPMH eka silicone gum), 175° x5minx15MPa


Swihlawulekisi swa Swikumiwa


Tipharamitha ta Xiendliwa .
Ximakiwa GA-9131
GA-9141 GA-9151 GA-9161 GA-9171
Xivumbeko Ku vonakala loku vonakaka
WilliamPlasticity .
120
140
200
240
270
Ku nonoka (ShoreA) .
30
40
50
60
70
Ku tsindziyela(g/cm3) . 1.11
1.14
1.17
1.18
1.19
Ku tiya ka ku koka (MPa) .

7.0
8.0
8.5
10.0
9.5
Ku leha(%) . 700
600
700
600
500
Matimba ya ku handzuka (kN/m) . 15
18
35
35
35
Ku tiya ka le henhla (Ω) .
1011


Hi nyika ku cinca loku heleleke ka GA-91X1 Antistatic Silicone Rubber, ku katsa na ku lulamisiwa ka ku tiya, ku tsindziyela, na swivumbeko swin’wana swa xiviri. Kunga khathariseki leswaku u lava swilaveko swo karhi swa matirhelo kumbe swihlawulekisi swo hlawuleka swa dizayini, ntlawa wa hina wa vativi wu lunghekele ku pfuneta hi swintshuxo leswi lulamisiweke eka phurojeke ya wena.


GA-91X1 Raba ya Silicone ya Antistatic


GA-91X1 Swihlawulekisi swa Raba ya Silicone ya Antistatic


GA-91X1 Antistatic Silicone Rubber, leyi nga na silica leyi khulukaka, yi nyika nsirhelelo wa kahle swinene wa electrostatic discharge (ESD) eka switirhisiwa swa elektroniki leswi nga na vuxiyaxiya.


Swihlawulekisi Swa Nkoka

  • Matirhelo yale henhla ya antistatic: Yinyika ku tiya ka le hansi ka le henhla eka vulawuri bya ESD lebyi tshembekaka eka switirhisiwa swa elektroniki.

  • A yi nun’hweli naswona yi hlayisekile: Yikahle eka ti indasitiri leti lavaka rhaba ya silicone leyinga riki na chefu, leyi hlayisekeke eka tindzhawu letinga na vuxiyaxiya.

  • Ku fambisana na RoHS na REACH: Yi fikelela swipimelo swa mbango eka milawu ya vuhlayiseki na tikhemikhali eka makete wa misava hinkwayo.

  • Ku tiya na ku olova: Matimba yale henhla ya tensile xikan’we naku leha switiyisisa leswaku switirhisiwa swa rhaba ya silicone switshama nkarhi woleha, hambi kuri eka swiyimo swo tika.


Swikombelo

  • Swiphemu swa elektroniki: Swi kahle ngopfu eka mavoko ya rhaba leyi nga cinciki, swirhendzevutana ni swilo swin’wana swa rhaba ya silicone leswi tirhisiwaka eka switirhisiwa swa elektroniki leswi nga ni vuxiyaxiya.

  • Switirhisiwa swo lwisana na static: Switirhisiwa ngopfu eka ti indasitiri leti lavaka swintshuxo swa rhaba leswi lwisanaka na static eka ku paka, ku hlayisa na ku khoma.


Swivutiso Ni Tinhlamulo Leti Vutisiwaka Nkarhi Na Nkarhi


Q1: Hi wihi matirhiselo yo sungula ya GA-91X1 Antistatic Silicone Rubber?
A1: Yi kahle swinene eka switirhisiwa swa elektroniki leswi nga na vuxiyaxiya bya ESD, ku fana na mavoko yo sirhelela na swirhendzevutani.


Q2: Xana rhaba ya silicone ya GA-91X1 yi fambisana na swipimelo swa vuhlayiseki swa matiko ya misava?
A2: Ina, yi fikelela ku landzelerisa ka RoHS na REACH eka milawu ya vuhlayiseki na mbango.


Q3: Xana ndzi nga endla rhaba ya silicone ya GA-91X1 hi ku landza swilaveko swo karhi?
A3: Ina, hi nyika swintshuxo leswi lulamisiweke ku fikelela vukulu bya wena byo hlawuleka, ku tiya, na swilaveko swa matirhelo.


Q4: Xana GA-91X1 yi nyika njhani swivumbeko swa antistatic?
A4: Xivumbeko xa rhaba na silica leyi khulukaka switiyisisa ku tiya ka le hansi ka le henhla eka nsirhelelo wo tshembheka wa ESD.


Q5: Xana GA-91X1 yi lulamerile ku tirhisiwa eka tindhawu to tika?
A5: Ina, ku tiya ka yona ni ku olova ka yona swi endla leswaku yi nga onhaki naswona yi tirha ehansi ka swiyimo leswi lavaka matimba.


Q6: Xana ndzi nga oda rhaba ya silicone ya GA-91X1 eka swiyimo swo hambana swa ku tiya?
A6: Ina, hi nyika swihlawulekisi swo tala swa ku tiya ku fambelana na swilaveko swo hambana swa xikombelo.


Q7: Hi tihi tiindasitiri leti nga vuyeriwaka eka rhaba ya GA-91X1 antistatic silicone?
A7: Yi tirhisiwa ngopfu eka tiindasitiri ta elektroniki, mimovha, na vumaki leti lavaka vulawuri bya static.


Q8: Xana GA-91X1 yi nga hoxa xandla njhani eka khwalithi ya swikumiwa na vuhlayiseki?
A8: Yi pfuneta ku hunguta ku onhaka loku fambelanaka na static, ku tiyisisa ku khomiwa loku hlayisekeke na ku pakiwa ka switirhisiwa swa elektroniki leswi nga na vuxiyaxiya.

Endzhaku: 
Landzelaka: 

XITLHOKOVETSELO XA XITLHANYI

SWILO SWA HINA

VUXOKOXOKO BYA VUXOKOXOKO

Engetelani: No.33, Lane 159, Gondzo ra Taiye, Xifundzha xa Fengxian, Shanghai
Riqingho / WhatsApp / Skype: +86 15221953351
Vukorhokeri bya Vutshila     2023 Shanghai Herchy Rubber Co., Ltd. Mepe wa sayiti |   Pholisi ya Vuhlayiseki | Nseketelo Hi Leadong.