Tel: +86 15221953351 E-mail: info@herchyrubber.com
Please Choose Your Language
thil siam chhuah te .
I awmna hmun: In » thil siam chhuah te . » Synthesis rubber 1000 a ni. » VMQ Silicone 1000 a ni. » GA-90×× Platinum catalyzed silicone rubber extrusion atan (HCR)

Loading a awm em?

Share to:
Facebook Sharing button a awm bawk.
Twitter atanga Sharing button a awm bawk.
Line Sharing button a awm bawk.
WeChat hmanga Sharing tih a ni.
LinkedIn Sharing button a awm bawk.
Pinterest hmanga Sharing tih a ni.
WhatsApp Sharing button 1000 a awm bawk.
ShareHe Sharing button hi a awm em?

GA-90×× platinum hmanga siam silicone rubber chu extrusion (HCR) atan hman theih a ni.

A hman dan: Hose, rubber strip,kitchenware, etc. siam chhuahna atan a tha. 
Thil pawimawh: Compression leh extrusion molding, transparence sang leh goodanti-yellowing property, non-toxic leh tasteless te hian ROHS, REACH, FDA leh LFGB te authentication an pass a.
  • GA-9041 a ni.

  • Herchy a ni a .

A awm theihna:
A tam ber:

Test: Platinum vulcanizing agent, 130°C x 5min x 15mpa.

Product Parameters 1000 a ni.
Thilsiam GA-9041 a ni.
GA-9051 a ni. GA-9061 a ni. GA-9071 a ni. GA-9081 a ni.
Landan Langtlang
Williamplasticity .
190
210
240
270
290
Harsatna (Shorea) .
40
50
60
70
80
Density(G/CM3) a ni. 1.13
1.16
1.18
1.19
1.21
Tensile chakna (MPA) .

9.0
10.0
10.0
9.5
9.0
Elongation(%) . 900
700
600
500
400
Tear chakna (kn/m) . 30
35
35
35
35










Hma chiah: 
Dawtchiah: 

Quick Links .

Contact information te .

Add: No.33, Lane 159, Taiye Road, Fengxian District, Shanghai-a awm chu a ni.
A rilru a buai em em a, a rilru a hah em em bawk a. +86 15221953351
e-mail hmangin:  info@herchyrubber.com
A rilru a buai em em a, a rilru a hah em em bawk a   .   2023 Shanghai Herchy Rubber Co., Ltd. Sitemap 100 a ni. |   Privacy Policy | 1000-in a thlawp a ni. Leadong 100 a ni..