GA-9041
Herchy
| Ku kumeka: | |
|---|---|
| Nhlayo: . | |
Xikambelo: xitirhisiwa xa vulcanizing xa platinum, 130°C x 5min x 15MPa.
| Tipharamitha ta Xiendliwa . | |||||
| Ximakiwa | GA-9041 |
GA-9051 | GA-9061 | GA-9071 | GA-9081 |
| Xivumbeko | Erivaleni | ||||
| WilliamPlasticity . |
190 |
210 |
240 |
270 |
290 |
| Ku nonoka (ShoreA) . |
40 |
50 |
60 |
70 |
80 |
| Ku tsindziyela(g/cm3) . | 1.13 |
1.16 |
1.18 |
1.19 |
1.21 |
| Ku tiya ka ku koka (MPa) . |
9.0 |
10.0 |
10.0 |
9.5 |
9.0 |
| Ku leha(%) . | 900 |
700 |
600 |
500 |
400 |
| Matimba ya ku handzuka (kN/m) . | 30 |
35 |
35 |
35 |
35 |