GA-6071AHT Silicone Rubber ku waya ya vvulovumenti eya waggulu ennyo (HCR)

GA-6071AHT Silicone Rubber ku waya ya vvulovumenti eya waggulu ennyo (HCR)
Okukozesa: kirungi okufulumya amaanyi aga kiragala vvulovumenti enkulu shielded cable, hightemperature-resistant cable, eggaali y'omukka transit cable, n'ebirala.
Ebintu ebikulu: okugoberera ebyetaago bya 1S06722-1 :2011 (E), GB / T33430-2016, ne LV 216;Excellent waggulu ne wansi temperatureresistance, obulungi extrusionprocessability,goodelectrical insulation property;Yayita okugezesebwa kw'ebbugumu okukaddiwa okumala 3000h, asobola okuwonyezebwa byombi DCBP ne platinum enkola.
  • GA-6071AHT

  • Herchy nga bwe kiri

Ebiriwo:
Omuwendo:

GA-6071AHT Silicone Rubber ku waya ya vvulovumenti eya waggulu ennyo (HCR)


Okukozesa: kirungi okufulumya amaanyi aga kiragala vvulovumenti enkulu shielded cable, hightemperature-resistant cable, eggaali y'omukka transit cable, n'ebirala.

Ebintu ebikulu: okugoberera ebyetaago bya 1S06722-1 :2011 (E), GB / T33430-2016, ne LV 216;Excellent waggulu ne wansi temperatureresistance, obulungi extrusionprocessability,goodelectrical insulation property;Yayita okugezesebwa kw'ebbugumu okukaddiwa okumala 3000h, asobola okuwonyezebwa byombi DCBP ne platinumsystem.

Okugezesebwa: pulatiniyamu A: 0.3%, pulatiniyamu B: 1.2%, 130°C x 5min.


CLASS E(180°C)Ebipimo by’ebintu
Ekyamaguzi GA-6071AHT GA-6071AHTAB
Endabika Etangalijja
Obuveera bwa William 265 265
Obukaluba (ShoreA) . 65 68
Obugumu(g/cm3) . 1.2 1.2
Amaanyi g’okusika (MPa) . 10 10.5
Okuwanvuwa(%) . 450 700
Amaanyi g’okukutuka (kN/m) . 33 45

Obuziyiza bwa voliyumu (Ω·cm) . 1.0*1015 1.0*1015

Amaanyi g’okumenya (kV/mm) . 25 25


Jjuuzi: 
Ekiddako: 

ENKOZESA Y'AMAWANGA

EBINTU EBYAFFE

AMAWULIRE AG'OKUKWATAGANA

Gattako: No.33, Lane 159, oluguudo lwa Taiye, mu Disitulikiti y’e Fengxian, Shanghai
Essimu / WhatsApp / Skype ku ssimu: +86 15221953351
Eddembe ly’okuwandiika     2023 Kkampuni ya Shanghai Herchy Rubber Co., Ltd. Sitemap y'ekifo |   Enkola y'Ebyama | Obuwagizi Bwa... Leadong.